Hastelloy C276(UNS N10276 W.Nr. 2.4819)
Collect
商品说明
Hastelloy C276(UNS N10276 W.Nr. 2.4819)1.Hastelloy C276 Introduction A nickel-molybdenum-chromium alloy with an addition of tungsten having excellent corrosion resistance in a wide range of severe environments. The high molybdenum content makes the alloy especially resistant to pitting and crevice corrosion. The low carbon content minimizes carbide precipitation during welding to maintain corrosion resistance in as-welded structures. Used in pollution control, chemical processing, pulp and paper production and waste treatment. 2.Hastelloy C276 MAJOR SPECIFICATIONS UNS N10276 ASTM B 366, B 462, B 564, B 574, B 575, B 619, B 622, B 626, B 751, B 775, B 829 DIN 17744, 17750 – 17754 Werkstoff Nr. 2.4819 VdTüV 400 ASME SB-366, SB-564, SB-574, SB-575, SB-619, SB-622, SB-626, SB-751, SB-775, SB-829 ASME Code Case 1924 NACE MR-0175/ISO 15156 ISO 6207, 6208, 9723 – 9725 3.Hastelloy C276 STANDARD PRODUCT FORMS Pipe, tube, sheet, strip, plate, round bar, flat bar, forging stock, hexagon and wire. 4.Hastelloy C276 LIMITING CHEMICAL COMPOSITION, %
5.Hastelloy C276 PHYSICAL CONSTANTS AND THERMAL PROPERTIES Density, Ib/in3 .........................................................................0.321 g/cm3 ......................................................................... 8.89 Melting Point, °F.....................................................2415 – 2500 °C.....................................................1325 – 1370 Specific Heat, Btu/lb •°F....................................................0.102 J/kg •°C.......................................................... 427 Coefficient of Expansion, 70 – 200°F, 10-6 in/in •°F........6.8 24 – 100°C, μm/m •°C......... 12.2 Thermal Conductivity, Btu • in/ft2• h•°F...........................67.9 W/m•°C.............................................9.8 Electrical Resistivity, ohm • circ mil/ft..........................739.2 μΩ•m..............................................1.229 Permeability at 200 Oersted (15.9 kA/m)................. 1.0002 6.Hastelloy C276 TYPICAL MECHANICAL PROPERTIES (Annealed) Tensile Strength, ksi............................................................... 100 MPa............................................................ 758 Yield Strength (0.2% Offset), ksi...........................................53 MPa..................................... 363 Elongation, % ..............................................................................62 |